I've been playing around with an alaskan 36 inch mill for the year and some of the wood has been getting blue mould. I dont have a kiln but have recently been put on to a chap who is running a home made one. Any tips on keeping this stuff away would be good as it isn't as nice to look at as a perfect grain. :confused1:

Link to comment
Share on other sites

Log in or register to remove this advert

  • Replies 22
  • Created
  • Last Reply

Top Posters In This Topic

The phenomenon that Hamadryad and Skyhuck are referring to is a dark blue/black stain within the wood, which is visible when you first mill it, formed by a reaction between the tannic acid present in some woods (notably oak and sweet chestnut) and iron, usually from nails or bits of fencing.

 

However, what you are referring to is called "blue stain" which is a mould growth on the surface fairly rapidly after milling. This is more likely to form on species without high tannin content.

 

There are several things you can do. First option is to paint everything with borate solution straight after milling. This is a durable inorganic fungicide, and stops the mould growing.

 

Second option which is a bit trickier is to mill only in clear, bright but cool weather - usually September through to April, and lay the boards out up off the ground out of direct sunlight, rather than stacking them immediately, turning every day or so. After a few days, time depending on temperature, light levels etc, you will see a subtle change in colour on the surface as they start to oxidise. In most pale species it's a slight yellowing; oak first loses that pinkish tinge, then goes very pale and then yellows a bit. If you stack the boards when they start to get that slight oxidation colour then they are much less wet at the surface and don't develop mould, however you have to be very careful to avoid either surface checking or case hardening in the process, which is why you have to keep them cool and in the shade.

 

Borate is much easier!

 

The other factor to consider is your stickers. They really do need to be very dry, as they will trap water against the surface of the board which then leads to local development of blue stain, known as sticker stain.

 

Hope this helps.

 

Alec

Link to comment
Share on other sites

The phenomenon that Hamadryad and Skyhuck are referring to is a dark blue/black stain within the wood, which is visible when you first mill it, formed by a reaction between the tannic acid present in some woods (notably oak and sweet chestnut) and iron, usually from nails or bits of fencing.

 

However, what you are referring to is called "blue stain" which is a mould growth on the surface fairly rapidly after milling. This is more likely to form on species without high tannin content.

 

There are several things you can do. First option is to paint everything with borate solution straight after milling. This is a durable inorganic fungicide, and stops the mould growing.

 

Second option which is a bit trickier is to mill only in clear, bright but cool weather - usually September through to April, and lay the boards out up off the ground out of direct sunlight, rather than stacking them immediately, turning every day or so. After a few days, time depending on temperature, light levels etc, you will see a subtle change in colour on the surface as they start to oxidise. In most pale species it's a slight yellowing; oak first loses that pinkish tinge, then goes very pale and then yellows a bit. If you stack the boards when they start to get that slight oxidation colour then they are much less wet at the surface and don't develop mould, however you have to be very careful to avoid either surface checking or case hardening in the process, which is why you have to keep them cool and in the shade.

 

Borate is much easier!

 

The other factor to consider is your stickers. They really do need to be very dry, as they will trap water against the surface of the board which then leads to local development of blue stain, known as sticker stain.

 

Hope this helps.

 

Alec

 

very informative post:001_cool:

Link to comment
Share on other sites

I've used wykabor for some time now:

 

http://www.wykamol.com/services/timber-treatment/wykabor-range/wykabor-powder.html]Wykabor Powder / Wykabor Range / Timber Treatments / Services / Wykamol Group / Specialist products for the building and preservation industries.

 

 

....and it's excellent. I'm sure that any borate would be fine though as it's all just Sodium tetraborate Decahydrate.

Link to comment
Share on other sites

Hi Rowan, you're talking about conifers and so the blue stain (if its blue stain fungi and not iron stain) would be associated with the sapwood. In conifers, Ceratocystis spp. are the usual culprits. The stain is not actually a 'stain' as such but is caused by the presence of dark (usually brown!) hyphae within the wood cells. These fungi are using the starch rich contents of the wood cells, rather than the cell walls themselves. Infection may occur prior to conversion, in which case there's not much you can do about it other than perhaps restrict it spreading. If it’s occurring at the point of conversion then as previous posts advise, you should look at the milling and storage environment. The fungi grow best in warm temperatures (20 deg C +). At 10 deg C or below growth is very slow. Timber moisture contents in excess of fibre saturation (say 28% w/w) are required; so rapid drying of fresh cut surfaces will go a long way to controlling blue stain. Rapid can achieve this. Kiln drying is the surest way to prevent fungal activity of any sort. However, it can be managed simply by the management of storage age and hygiene

The financial loss due to blue stain fungi and significant the world over. There is no shortage of academic study and industrial collaborations to address the matter. Alec has already given you some sound practical advice

I’ll make another post with some opinion on the use of Boron/ Borax etc. I hope not to sound like an activist (because I’m not one honest!); I’m no expert; however, I’ve been commercially / professional involved in the subject for over 25 yrs and thats slowly formed my views on the matter

cheers

Pete

Link to comment
Share on other sites

Rowan,

Chemical surface treatment is widely used on green timber. Boron in the form Sodium Octaborate Tetrahydrate is commonly used at 5% - 10% and is effective. However, consider this: you are introducing a pesticide into the production of a natural material. Boron wood preservatives have just had to be re-classified in the EU as 'Toxic' because of evidence related to mammalian toxicity ability to cross the placenta and an association with male infertility). Formerly they were classified in the UK as 'Hazardous' and I can remember when they were introduced for preservative wood treatment in the UK in the 1980's they were widely billed as 'green' or 'environmentally friendly' etc. Whilst this may be the logical option for you, you should in my view consider that boron is not chemically fixed to the timber following application. So wetting may leach it out. Where does it go? Also, when the wood is further milled, what happens to the waste? It now contains a pesticide. I'm not advising that you don’t use boron (I very occasionally I specify it myself) and its true that some timbers are at least as ‘toxic’ in the context. However, it’s important to only employ it where there is no other practical option; and if you do use it you should look at the wider ‘life cycle’ of the product (i.e. where does it go to eventually)

There has been a suggestion that a broad-spectrum pesticide is used. E.g. one that kills both insects and fungi. There’s a simple rule when using pesticides (and it is part of your statuary obligations) and that is to target the pest. If the problem is fungal then that’s the target. Woodworm (insects) are not the target. Broad-spectrum wood treatments will usually contain more than one pesticide. For Woodworm Permethrin or Cypermethrin are often found in formulations. Both are extremely toxic in aquatic environments and so you must consider what happens to run-off and to waste.

cheers

Pete

Link to comment
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
 Share


  •  

  • Featured Adverts

About

Arbtalk.co.uk is a hub for the arboriculture industry in the UK.  
If you're just starting out and you need business, equipment, tech or training support you're in the right place.  If you've done it, made it, got a van load of oily t-shirts and have decided to give something back by sharing your knowledge or wisdom,  then you're welcome too.
If you would like to contribute to making this industry more effective and safe then welcome.
Just like a living tree, it'll always be a work in progress.
Please have a look around, sign up, share and contribute the best you have.

See you inside.

The Arbtalk Team

Follow us

Articles

×
×
  • Create New...

Important Information

We have placed cookies on your device to help make this website better. You can adjust your cookie settings, otherwise we'll assume you're okay to continue.